WL 1.3514-100 Aerospace series - Chromium ball and roller bearing steel with approx 1 C - 1,5 Cr, consumable electrode remelted - Part 100: Bar, wire, forging and tubing - Notes for design and production, cross-reference. Формат поставки-PDF. Язык стандарта-Немецкий
Другие Стандарты WL
WL 1.7220 Heat-treatable chromium-molybdenum steel with about 0,35C-1Cr-0,2Mo; rods and wire for screws ...
WL 1.4974-1 Precipitation-hardening high temperature chromium-nickel-cobalt steel with about 0.1C-21Cr-20Ni-19Co; s...
WL 1.4928-1 Aerospace series - High-temperature chromium-nickel-molybdenum-cobalt steel casting with ...
WL 1.4956 Precipitation-hardening high temperature chromium-nickel-cobalt steel with about 0.08C-21Cr-20Ni-19Co; ...
WL 1.6359-2 Beiblatt 1 Ultra high-strength maraging nickel-cobalt-molybdenum steel with about 0.01 C...
WL 1.4581 Beiblatt 1 Stainless austenitic chromium-nickel-molybdenum cast steel with about 0.06C-1...